super alloy 5 aluminum boat repair
The seam that runs down this aluminum boat has separated and is leaking badly. to make the repair, we use super alloy 5 and an oxyacetylene torch to seal the area that had been unsuccessfully. Always clean the aluminum with an abrasive such as a sanding disk, wire wheel etc prior to brazing with super alloy 5, to remove oxidation and impurities from the parent metal.. Split seams on aluminum boats is a common problem. while many boat owners resort to temporary fixes such as epoxy, super alloy 5 is a permanent repair for aluminum boat seams. in this video, an aluminum boat with a separated seam is repaired quickly and easily, using super alloy 5 and an oxyacetylene torch. oxyacetylene, oxy-mapp gas, or oxy.
super alloy 5 aluminum boat repair Step by step instructional video for how to repair damaged aluminum boat propellers with super alloy 5 aluminum welding rod. note that an oxyacetylene or other oxygen-fueled torch is required when working on any aluminum boat or large mass of aluminum. propane torches will not heat the parent metal to a proper working temperature.. Super alloy 5 aluminum brazing rod and an oxyacetylene torch with size 1 brazing tip are used to repair a large dent in an aluminum boat. for this application, a carburizing flame is recommended, to avoid overheating the thin aluminum parent metal..
Comments
Post a Comment